The two grades look the same on the shelf and behave very differently five years in. Here is how to choose between them without over- or under-specifying — and how to verify you got what you paid for.
12 min read · By Alwin Pan, Overseas Business Director, Haoyue Metal
Grade selection is one of the most common places an order goes wrong. A buyer saves on material, the doors go into a humid or coastal site, and the rust appears after installation — when replacement costs many times the original saving. This guide explains the real difference, how to read the test data, and how to confirm the grade on an incoming shipment.
Both 201 and 304 are stainless steels, and both look bright when new. The difference is the alloy: 304 contains roughly 18% chromium and 8% nickel; 201 substitutes some of that nickel with manganese and nitrogen. The result is that 304 resists corrosion significantly better, especially in wet or salty air, while 201 is cheaper. The nickel is what you are paying for, not the polish.
| Property | 201 | 304 |
|---|---|---|
| Alloy | ~16–18% Cr, low Ni, Mn + N substituted[1] | ~18% Cr, ~8% Ni[1] |
| Corrosion resistance | Moderate — fine in dry interiors | High — suitable for wet and coastal sites |
| Salt spray (indicative) | Rust often within tens of hours | 72 h or more with no marked change |
| Forming | Higher strength, lower elongation — can crack in deep draws[2] | Better ductility, easier deep drawing and bending[2] |
| Cost | Lower | Higher |
| Typical use | Furniture, interior doors, dry cabinets | Bathrooms, kitchens, marine, wash-down |
A useful technical measure is the pitting resistance equivalent number, PREN = %Cr + 3.3×%Mo + 16×%N. 304 sits around 18–20; 201 around 14–16. Each point matters in chloride environments such as coastal air[2]. What that means in practice: an uncoated 201 bracket near the sea can show visible rust within half a year to a year, while 304 commonly stays sound for several years.
Bedroom furniture, office cabinets, interior doors. 201 is adequate and saves money with no practical loss of performance.
Bathrooms, laundries, sea-side properties, commercial kitchens. Specify 304 — the extra cost is small compared with replacing rusted hinges and the labour to do it.
Wash-down environments and equipment cleaned with chemicals. 304 is the usual minimum; some specifications call for 316. Confirm with your customer.
A common buying mistake is to treat the choice as either "always 304" or "cheapest possible". The right answer follows the environment. Price the whole life of the installed hinge, not just the purchase order — sanding, repainting, replacement parts and call-outs usually cost more than the material saving.
Salt spray hours are often quoted as if they were a score. They are not comparable unless four things are stated: the standard (ASTM B117 and GB/T 2423.17 are common), the pass criterion (first rust, red rust, or no visible change), the sample state (bare, passivated or coated; flat coupon or finished part), and the environment behind the number[3]. A flat passivated coupon will always outperform a finished hinge with bends and welds.
The standard number, the criterion, the sample description and the test report — all four. If a supplier gives a bare "72-hour salt spray" claim and cannot say what was tested, treat it as an adjective rather than data.
Our hinges are tested to 72 hours of neutral salt spray. We state the standard and the criterion on request, and the test is run on the finished part rather than a polished coupon, because that is what the customer installs.
Ask for the mill certificate, and ask whether the heat or lot number on it follows the order through production. We buy strip to the grade written on the drawing — SUS304, SUS201 or SPCC — keep the certificate and delivery note on file, and record the lot number so a finished hinge can be traced back to its strip. A supplier who cannot show this is asking you to take the grade on trust.
| Method | Reliability | What it can and cannot tell you |
|---|---|---|
| Marking / certificate | High, first check | SUS304, A2-70, A4-80 etc. plus a mill certificate with heat number. Vague "stainless steel" needs questioning.[4] |
| Magnet | Low, rough screen only | Both grades are weakly magnetic after forming; it cannot reliably separate 201 from 304. It is useful for spotting zinc alloy or plain iron. |
| Acid test liquid | Broad screening only | Separates the 200 and 300 series roughly, cannot name a grade, and its strong acid damages the passive layer — avoid on finished parts.[4] |
| Handheld XRF | High, quantitative | Reads chromium, nickel and manganese directly in seconds, non-destructively. The accepted method for incoming inspection of critical parts.[1] |
For coastal, food or medical projects, combine all of it: approve the certificate, screen a sample, and use XRF or a third-party lab report on the delivered batch. Put the grade and the verification method into the purchase order so there is something to hold against.
304 has about 18% chromium and 8% nickel. 201 replaces part of the nickel with manganese and nitrogen — cheaper, but less corrosion-resistant. In salt spray, 201 often rusts within tens of hours while 304 withstands 72 hours or more; 304 also forms and welds better.
For dry indoor furniture, yes. For bathrooms, coastal properties, commercial kitchens and wash-down areas, specify 304 — the saving is quickly lost to rust and replacement labour.
Only as a rough screen. Cold forming introduces magnetism in both grades, so the result is unreliable. Acid test liquids only separate the series broadly and can damage the passive layer. The mill certificate or XRF analysis is the proof.
Ask for the standard, the pass criterion, the sample state and whether humidity was included. A bare "72-hour" claim without those four things is an adjective, not data.
Ask for the mill certificate with heat/lot number tied to your order. For critical projects use handheld XRF on the finished part, or a third-party lab report. We keep certificates and lot numbers for every run.
In a dry interior, no — 201 or plated steel does the job. In a wet, salty or chemically cleaned environment, one replacement visit usually costs more than the material difference across the order.
Technical figures here are cited to published sources. Our own material certificates and in-house test data are available on request for any production run.